GH4169 Nickel-based Superalloy Metallographic Preparation

GH4169 nickel-based superalloy is widely applied in hot-section components of aero-engines, as well as high-temperature load-bearing structural parts for aerospace and energy industries.

Metallographic inspection plays a vital role. It visually evaluates grain size, gamma prime precipitation and harmful phase distribution, closely correlating with material strength, creep and fatigue properties.


Strict specimen preparation is required. Samples are ground progressively to eliminate scratches, then finely polished with diamond and oxide suspensions to achieve deformation-free mirror surface. Proper pressure and duration control prevent artificial defects, delivering authentic test data for process optimization and quality assessment.

3 (23)
3 (23)
4 (20)
4 (20)

Polishing Procedure

● P180 abrasive paper with water cooling

● POS disc + 9μm PD-WT suspension

● YS-JP disc + 3μm PD-WT suspension

● ET-JP disc + 50nm SO-A439 suspension

Step 2 can be replaced with P400, P800, P1200 or P2000 abrasive paper

2 (26)
2 (26)
1 (40)
1 (40)
prev
Electrolytic Etching Solution for Welded 304 Stainless Steel Specimens
Metallographic Examination of Al‑Sc Alloys
next
recommended for you
Get in touch with us
Contact Person: Sophy Liu
Tel: +86-(0512) 6528 3666
Email: info@trojanchina.com
WhatsApp: +86 133 82101195
Address: Building 26, No. 228 Gongtang Road, Luzhi Town, Wuzhong, Suzhou, Jiangsu, China
Product Lives
Customer service